Material Testing Technology Co.     |   home
SACM.00188.12   |   SACM.00288.20   |   SACM.00388.30   |   SACM.00689.10   |   SACM.00989.10
SACM.00288.20
SACMA METHOD - COMPRESSION-AFTER-IMPACT FIXTURE(S.S.)

Model No. SACM.00288.20

Specimen:



Fixture:
Width
Thickness
Length

Construction
Temperature
Mounting

Capacity
Weight
Dimensions
Standard
4.000” ±0.005”
0.100” to 0.375”
6.000” ±0.005”

17-4 series stainless steel
-240°F (-150°C) to 600°F (316°C)
Bottom - platen
Top - custom adapter or platen
50,000 lb. (222 kN)
30 lb. Approximately
Assembled - 3” x 8” X 14”
Manufactured and sold in accordance with:
SACMA Recommended Method SRM 2-88


      MATERIAL TESTING TECHNOLOGY  
1676 S. Wolf - Wheeling, IL  60090  Phone: (847) 215-7448   Fax: (847) 215-7449
---------------------------------------------------------------------------------------------------------------------------------
© Copyright 2003 - Material Testing Technology